Return to Technical Support

Technical Bulletin Regarding the Density of Glycerol in DROPimage Advanced

Sept 2025

It appears that there was an error that was introduced to our liquids.txt file in our DROPimage Advanced Software. The error relates the density of glycerol. If you are running DROPimage Advanced and would like to check to see if this error affects your installation, follow these steps:

1. In DROPimage Advanced, click on Edit > Edit Phase Data.

2. Change the Phase File to "Liquids".

3. Scroll down to "Glycerol". If the value reads 1.26, you're good to go.

4. If a different value is reported, then change it to 1.26, click on Save, and then Click on Close. You are now good to go.

We'd like to thank our customers at Argonne National Lab for finding the error.

If you require any additional technical assistance, please contact us with your serial number and the nature of your inquiry.
 

For more information or a quotation, please contact us
or call 973-448-0305
©2025, ramé-hart instrument co. All rights reserved.